详细说明
Thermanit 25/35 R Classifications EN 1600 Mat. No.
E Z25 35 Nb B 2 2 1.4853
说明: Resistant to scaling up to 1050 °C (1922 °F).
For surfacing and joining work on matching/similar heat
resistant cast steel grades.
对扩大到1050°C(1922°F)。
堆焊和加入工作匹配/类似的热
耐铸钢的成绩。
用途: TüV certified parent metal
GX40NiCrNb35-25 (1.4852)
熔敷金属化学成分(%)C Si Mn Cr Ni Nb
0.40 1.0 1.8 25.0 35.0 1.3
熔敷金属力学性能Heat- Yield strength Yield strength Tensile Elongation
treatment 0.2% 1.0% strength (L0=5d0)
N/mm2 N/mm2 N/mm2 %
AW 400 450 600 8
参考电流 (AC、DC+)Packaging, weights
and amperages
Dimensions (mm) pcs./pack kg/pack Amperage A
2.5 x 300 210 3.8 55- 80
3.2 x 350 130 4.2 80-105
4.0 x 350 94 4.6 90-135 |
|